MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Saint-Gobain CHR® M823 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape
Categories: Polymer; Adhesive; Tape; Thermoset; Silicone

Material Notes: CHR® M-Series (1 Mil PET/Silicone Adhesive) is manufactured from polyester film with silicone pressure-sensitive adhesive.

Features/Benefits: M823 is recommended for all splicing applications including oven splicings where good wet-out capabilities are critical. Polyester backing resists damage from sharp edges. The polyester backing/silicone adhesive combination is highly conformable. Operating temperature is -73 to +177 °C, elongation % at break is 100, tensile strength is 44 N/cm and dielectric strength is 5,000 volts.

Applications: M823 is designed as a quick-stick polyester splicing tape most often used in the graphic arts industry.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 100 %
Tear Strength 25.0 pliInitial Tear Strength
Peel Strength 0.330 kN/mAdhesion to Steel
 
Electrical PropertiesOriginal ValueComments
Dielectric Breakdown 5000 V
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 350 °F
Minimum Service Temperature, Air -100 °F
 
Descriptive Properties
ColorBlue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Daikin NEOFLON® NF-1500 FEP Film
3M 966 Adhesive Transfer Tapes with Adhesive 100

PSTGQZ318 / 68832

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.