MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mueller Dynalloy Alloy 6730 Free cutting bearing bronze (UNS C67300)
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Free cutting bearing bronze

Applications: Dynalloy is widely used for bearing applications, bushings, gears, valve guides, shaft and cylinder guides. The alloy has found wide acceptance in speed reducer gears and is an excellent alloy for axial piston pump components.

Information Provided by Mueller Industries Inc.

Key Words: UNS C67300, SAE J463, C6730 (Rods, Bars, Shapes and Forgings)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.50 g/ccBased on UNS number
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 86
Tensile Strength at Break 85000 psi
Tensile Strength, Yield 66000 psi
Elongation at Break 16 %
Machinability 70 %UNS C36000 = 100%
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 59.5 %
Lead, Pb 1.0 %
Manganese, Mn 2.5 %
Silicon, Si 1.0 %
Zinc, Zn 36 %Remainder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Manganese Brass, UNS C67300
High-Leaded Tin Bronze, UNS C93200, Copper Casting Alloy, Bearing Bronze SAE 660
Tin Bronze UNS C90300, Copper Casting Alloy
Ampco Metal AMPCO® 673 Manganese Bronze
MetalTek Bearium® B-4 Bearing Bronze

NMUEL909 / 97697

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.