MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CHT Group QM True Skin 50 Addition Cure Material, 50 Shore OO
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: QM True Skin 50 is a two-component, one-to-one mix ratio, heat cured, addition cure, silicone material. The cured rubber is very soft, has excellent mechanical properties, low fluid bleed and good shelf-life stability. This material is an outstanding choice for skin molding and applications where a low durometer and high elongation, translucent material is required.

Key Features:

  • Low viscosity
  • High elongation
  • Excellent toughness
  • Fast demold time
  • Translucent and pigmentable
Main Applications:
  • Special effects
  • Skin replication
  • Applications where pigmentation is required

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccUncatalyzed, QM True Skin 50 A
 1.05 g/ccUncatalyzed, QM True Skin 50 B
Viscosity 15000 cPUncatalyzed, QM True Skin 50 A
 15000 cPUncatalyzed, QM True Skin 50 B
Linear Mold Shrinkage <= 0.0010 cm/cmCured 30 minutes at 90°C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore OO 48Cured 30 minutes at 90°C
Tensile Strength 325 psiCured 30 minutes at 90°C
Elongation at Break 835 %Cured 30 minutes at 90°C
Tear Strength 30.0 pliCured 30 minutes at 90°C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204 °CCured 30 minutes at 90°C
Minimum Service Temperature, Air -55.0 °CCured 30 minutes at 90°C
 
Processing PropertiesOriginal ValueComments
Cure Time >= 30.0 min
@Temperature 90.0 °C
As Tested
Gel Time 105 minCatalyzed, QM True Skin 50
 
Descriptive Properties
ColorTranslucentUncatalyzed, QM True Skin 50 A
 TranslucentUncatalyzed, QM True Skin 50 B
 TranslucentCatalyzed, QM True Skin 50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CHT Group True Skin® 30 30 Shore A, Clear Addition Cure Material
Dow HV 1650/50 SILICONE RUBBER
Wacker Elastosil® R 701/50 Silicone Rubber
CHT Group QM 254 60 Shore A, Addition Cure Moldmaking Material
CHT Group QLE 1037 60 Shore A, Addition Cure Elastomer for Coating Applications

PACC2075 / 199463

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.