MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CeramTec Frequenta® Steatite
Categories: Ceramic; Oxide; Magnesium Oxide; Silicon Oxide

Material Notes: Steatites used in place of aluminas are a cost-effective way to meet performance requirements. They are easier to form and fire at lower temperatures. Frequenta® has low dielectric loss, but has been developed for superior strength and low thermal conductivity for higher temperature applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.80 g/ccDIN EN 623-2 / ASTM-C373 / ASTM-C20
Water Absorption 0.00 %DIN EN 623-2 / ASTM-C373
 
Mechanical PropertiesOriginal ValueComments
Tensile Modulus 120 GPaYoung's; DINV ENV 843-2 / ASTM-F417
Compressive Strength 900 MPaASTM C-773-88 / DIN 51067T1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+7 ohm-cm
@Temperature 500 °C
 1.00e+13 ohm-cm
@Temperature 100 °C
IEC 672-1
Dielectric Constant 6.0
@Frequency 1e+6 Hz
IEC 672-1 / ASTM-C150
Dielectric Loss Index 0.0012
@Frequency 1e+6 Hz
IEC 672-1 / ASTM-D149,150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.00 - 8.00 µm/m-°C
@Temperature 20.0 - 200 °C
 7.00 - 9.00 µm/m-°C
@Temperature 20.0 - 600 °C
ASTM-C373
 8.00 - 9.00 µm/m-°C
@Temperature 20.0 - 1000 °C
Specific Heat Capacity 0.850 J/g-°C
@Temperature 100 - 200 °C
DINV ENV 821-3
Thermal Conductivity 2.50 W/m-KDIN EN 821-2 / ASTM-C408
Maximum Service Temperature, Air 1000 °C
 
Descriptive Properties
ColorBuff
Thermal Shock Resistance R1 (K)160Hasselman (Experimental)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Frequentite 1000 Steatite
Du-Co Ceramics DC-10-L-3 Steatite
Du-Co Ceramics DC-16-L-3 Steatite
Du-Co Ceramics DC-9-L-3 Steatite
Du-Co Ceramics CS-144-L-5 Steatite

CCERA924 / 107524

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.