MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

(Viewing data as-entered. Click here to return)
Cookson Group Plaskon® LS-16 Low Stress Epoxy Molding Compound  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Molding Compound

Material Notes: This material is a low stress molding compound specifically formulated for use with automated molding equipment to increase semiconductor manufacturing productivity and reduce production costs. This compound is recommended for molding of stress sensitive DIPs, SOICs, PLCCs and small QFPs.

Features:

  • Consistent, expedient moldability
  • Broad range of molding temperatures
  • Fast cycle times
  • Low viscosity
  • Minimal post mold cure
  • Low stress

Information provided by Cookson Electronics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.83 g/cc
Viscosity 1800 cP
@Temperature 165 °C
Automatic orifice
Spiral Flow 51.0 cmat 165°C and 1000 psi
Ash 74.2 %
Storage Temperature <= 5.00 °CRecommended
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80Cull hot, 75 sec @ 165°C
Flexural Strength 16000 psi
Flexural Modulus 1.700e+6 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 9.50e+15 ohm-cm
Dielectric Constant 3.3
@Frequency 1000 Hz
Dielectric Strength >= 400 V/mil
Dissipation Factor 0.00030
@Frequency 1000 Hz
Arc Resistance >= 180 sec110V AC
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.9 µm/m-°C
@Temperature 20.0 °C
Alpha 1, 2 hr post cure
 16.5 µm/m-°C
@Temperature 20.0 °C
Alpha 1, 15 min post cure
 16.7 µm/m-°C
@Temperature 20.0 °C
Alpha 1, as molded
 61.0 µm/m-°C
@Temperature 20.0 °C
Alpha 2, as molded
 65.0 µm/m-°C
@Temperature 20.0 °C
Alpha 2, 15 min post cure
 66.0 µm/m-°C
@Temperature 20.0 °C
Alpha 2, 2 hr post cure
Thermal Conductivity 0.657 W/m-K2 hr post cure, 175°C
Glass Transition Temp, Tg 150 °C
 160 °C15 min post cure
 162 °C2 hr post cure
Flammability, UL94 V-0
@Thickness 3.17 mm
Oxygen Index 30 %
 
Processing PropertiesOriginal ValueComments
Mold Temperature 165 - 175 °C
Back Pressure 500 - 1000 psi
Cycle Time - Injection 30 - 40 secat 165-175°C
Cure Time 0.000 - 0.250 hour
@Temperature 165 - 170 °C
Post mold
Gel Time 0.233 minRam follower, at 165°C
Shelf Life 0.0670 Monthat 35°C, <40% loss of spiral flow
 0.167 Monthat 21°C, <40% loss of spiral flow
 24.0 Monthat 5°C, <40% loss of spiral flow
 
Descriptive Properties
Hydrolyzable Cl<1 ppm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cookson Group Plaskon® MUF-2A LAR Molded Underfill Compound for Flip Chip BGAs and CSPs
Overview of materials for Epoxy Molding Compound
Cookson Group Plaskon® CMU-870-2C Molded Underfill Compound for Flip Chip BGAs and CSPs
Cookson Group Plaskon® CMU-870-2B Molded Underfill Compound for Flip Chip BGAs and CSPs
Cookson Group Plaskon® CMU-870-2A Molded Underfill Compound for Flip Chip BGAs and CSPs

PPLASK020 / 56310

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.