MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema Kynar® UHM 6020-20 PVDF-GF
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF)

Material Notes:

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.87 - 1.89 g/ccASTM D792
Water Absorption 0.00 %Dry; Sim. to ISO 62
Moisture Absorption 0.000 %Dry; Sim. to ISO 62
Linear Mold Shrinkage 0.0025 - 0.010 cm/cmat 50% RH; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 120 MPaDry; ISO 527-1/-2
Tensile Strength, Yield 120 MPaASTM D638
Elongation at Break 3.0 %ASTM D638
 3.0 %Dry; ISO 527-1/-2
Tensile Modulus 788 MPaASTM D638
 7900 MPaDry; ISO 527-1/-2
Flexural Strength 174 MPa
@Strain 5.0 %
ASTM D790
Flexural Modulus 6560 MPaASTM D790
Izod Impact, Notched 101 J/mASTM D256
Charpy Impact Unnotched 44.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eU
Tensile Creep Modulus, 1 hour 7900 MPaCond.; ISO 899-1
Tensile Creep Modulus, 1000 hours 7900 MPaCond.; ISO 899-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 35.0 µm/m-°CDry; ISO 11359-1/-2
CTE, linear, Transverse to Flow 35.0 µm/m-°CDry; ISO 11359-1/-2
Melting Point 165 - 172 °CASTM D3418
 170 °C10°C/min; Dry; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 160 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 159 °CASTM D648
 159 °CDry; ISO 75-1/-2
Flammability, UL94 V-0IEC 60695-11-10
 
Processing PropertiesOriginal ValueComments
Melt Temperature 230 °CInjection Molding; ISO 294
 230 - 250 °C
Mold Temperature 20.0 - 60.0 °C
 60.0 °CInjection Molding; ISO 10724
 
Descriptive Properties
Form as DeliveredPellets
Moisture SensitiveNo
Processing MethodsInjection Molding
 Profile Extrusion
 Transfer Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Arkema KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
3M Dyneon™ PVDF 6008/0001 Polyvinylidene Fluoride
Arkema Kynar® 340 PVDF-CD
Arkema KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding

PARKF754 / 193546

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.