MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Parker Chomerics V-THERM™ Thermally Conductive Elastomer  (discontinued **)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: V-THERM thermally conductive elastomer interface pads are designed for use between heat generating components and cooling devices. This material conforms to surface irregularities under moderate application pressures to fill air gaps between components and their heat sinks.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/ccASTM D792
Deformation 10 %
@Thickness 1.52 mm,
Pressure 0.689 MPa
 12 %
@Thickness 1.02 mm,
Pressure 0.689 MPa
 16 %
@Thickness 1.02 mm,
Pressure 1.38 MPa
 16 %
@Thickness 1.52 mm,
Pressure 1.38 MPa
 48 %
@Thickness 1.02 mm,
Pressure 2.76 MPa
 49 %
@Thickness 1.52 mm,
Pressure 2.76 MPa
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 25ASTM D2240
Compression Set 80 %
@Temperature 125 °C,
Time 79200 sec
ASTM D395
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.00e+14 ohm-cmASTM D257
Dielectric Constant 2.9
@Frequency 100 Hz
ASTM D150
 3.3
@Frequency 100 Hz
ASTM D150
Dielectric Strength 150 V/milASTM D149
Dissipation Factor 0.0013
@Frequency 100000 Hz
ASTM D150
 0.023
@Frequency 100 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 5.00 W/m-K
@Thickness 0.510 mm
ASTM D5470
 6.00 W/m-K
@Thickness 1.02 mm
ASTM D5470
 7.00 W/m-K
@Thickness 1.52 mm
ASTM D5470
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -60.0 °C
 
Descriptive Properties
BinderSilicone
CarrierNone
ColorBlue
FillerBoron Nitride

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Parker Chomerics CHO-THERM 1641 Thermally Conductive Silicone
Celanese CoolPoly® E5105 Thermally Conductive Polyphenylene Sulfide
Celanese CoolPoly® E5103 Thermally Conductive Polyphenylene Sulfide
Celanese CoolPoly® E4501 Thermally Conductive Polycarbonate
Celanese CoolPoly® E4301 Thermally Conductive Polybutylene Terephthalate

PCHOME002 / 28224

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.