MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC NORYL PPX™ Resin PPX640F Polyphenylene Ether + PP (PPE+PP)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polypropylene (PP)

Material Notes: NORYL PPX™ 640F resin is a 40% glass reinforced alloy of polyphenylene ether (PPE) + polypropylene (PP). This injection moldable grade is NSF 61 certified and exhibits high elongation and stiffness along with temperature performance, impact resistance, hydrolytic and dimensional stability. NORYL PPX640F resin is an excellent candidate for copper and brass replacement in water management applications such as water filtration systems, boiler systems, and heat exchangers.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,Good Stiffness,Low Warpage,Food Contact Acceptable,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccASTM D792
Moisture Absorption 0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0017 - 0.0018 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0027 - 0.0061 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 1.3 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 95.0 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 95.0 MPa5 mm/min; ASTM D638
Elongation at Break 6.4 %5 mm/min; ASTM D638
Flexural Strength 150 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 8310 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 106 JASTM D256
 96.0 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched 576 J/mASTM D4812
Dart Drop, Total Energy 16.0 JASTM D3763
 14.0 J
@Temperature -30.0 °C
ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 10.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 63.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 158 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 146 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 163 °CRate B/50; ASTM D1525
Flammability, UL94 HB
@Thickness >=1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 260 - 305 °C
Zone 2 250 - 290 °C
Zone 3 255 - 300 °C
Melt Temperature 260 - 305 °CInjection Molding
Mold Temperature 40.0 - 65.0 °C
Drying Temperature 65.0 - 75.0 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 30 - 70 %
Vent Depth 0.00510 - 0.00760 cm
Screw Speed 20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82215 / 290162

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.