MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Lord Adhesives CoolTherm™ SC-322 Thermally Conductive Adhesive
Categories: Polymer; Thermoset; Silicone; Silicone Elastomer, for Thermal Management

Material Notes: LORD CoolTherm™ MT-322 thermally conductive adhesive is a one-component silicone adhesive designed for use in assemblies where thermal dissipation is desired. CoolTherm MT-322 adhesive can be used to bond electronic devices such as memory chips to lids, heat spreaders and heat sinks. The adhesive cures to form a flexible elastomer offering superior high temperature electrical properties.

Features: exhibits low shrinkage and stress on components as it cures. composed of an addition-curing polydimethyl siloxane polymer that will not depolymerize when heated in confined spaces. provides excellent adhesion to a wide variety of surfaces including silicon, ceramic, plastic and metal. can be used on parts and devices that experience operating temperatures from -40°C to +200°C.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.65 g/cc
@Temperature 25.0 °C
Viscosity 65000 cP
@Temperature 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 65cured; ASTM D 2240
Shear Strength 305 psiLap Shear, cured; ASTM D 1002
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+14 ohm-cm
@Temperature 25.0 °C
cured; ASTM D 257
Dielectric Constant 2.9
@Frequency 1e+6 Hz
cured; ASTM D 150
Dielectric Strength 254 V/mil
@Temperature 25.0 °C
cured; ASTM D 149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 160 µm/m-°Ccured; ASTM D 864
Thermal Conductivity 1.70 W/m-Kcured, mathis hot disk
Crystallization Temperature -47.0 °Ccured
Maximum Service Temperature, Air 200 °C
Minimum Service Temperature, Air -40.0 °F
 
Processing PropertiesOriginal ValueComments
Pot Life 1.00 min
@Temperature 25.0 °C
month, working life
Shelf Life 6.00 Month
@Temperature 5.00 °C
from date of manufacture when stored in original, unopened container
 
Descriptive Properties
AppearanceGrey Paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lord Adhesives CoolTherm™ SC-324 XLW Thermally Conductive Silicone Encapsulant
Lord Adhesives CoolTherm™ SC-324 Thermally Conductive Epoxy Encapsulant
Lord Adhesives CoolTherm™ SC-320 THK Thermally Conductive Silicone
Lord Adhesives CoolTherm™ SC-320 Thermally Conductive Silicone Encapsulant
Lord Adhesives CoolTherm™ SC-320 SLW Thermally Conductive Silicone Encapsulant

PLORD9238 / 232594

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.