MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MetalTek MTEK 316 Cast UNS J92900 Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; Cast Stainless Steel; T 300 Series Stainless Steel

Material Notes: "300" series, general corrosion resistant alloy

Applications: Nuclear, chemical and food processing. Valve and pump trim.

Information provided by MetalTek

Key Words: Cast UNS J92900; Cast Grade CF8M; Cast ASTM A351, A743, A744; AMS 5361 (Centrifugal Casting); Wrought UNS S31600; Wrought Grade 316
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 179179
Tensile Strength, Ultimate >= 485 MPa>= 70300 psi
Tensile Strength, Yield >= 205 MPa>= 29700 psi
Elongation at Break >= 30 %>= 30 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.080 %<= 0.080 %
Chromium, Cr 18 - 21 %18 - 21 %
Iron, Fe 60.92 - 71 %60.92 - 71 %As Balance
Manganese, Mn <= 1.5 %<= 1.5 %
Molybdenum, Mo 2.0 - 3.0 %2.0 - 3.0 %
Nickel, Ni 9.0 - 12 %9.0 - 12 %
Silicon, Si <= 1.5 %<= 1.5 %
 
Descriptive Properties
Heat TreatmentSol. Anneal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cast Stainless Steel CF8M, ASTM A351
Cast Stainless Steel CF8M, UNS J92900
Cast Stainless Steel CF8M, ASTM A743
Cast Stainless Steel CF8M, ASTM A744
Cast Stainless Steel CF8M, ACI

NMETEK046 / 18296

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.