MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

3D Systems Accura® 10 Plastic for SLA® Systems
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Accura 10 "Nd" type material - for use with Viper SLA, and SLA 3500, 5000 and 7000 systems.

    Applications
  • General use prototyping for many uses, including:
    • Enclosures, covers and cases
    • Cellular/mobile phones
    • Automotive and aerospace design
    • Computers and control displays
  • Accurate master patterns for RTV/silicone molding
  • QuickCast™ patterns for investment casting
  • Models for fluid flow and visualization of internal structures

All information provided by 3D Systems.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.


Axis Proto Inc. Industry leaders in providing high quality Rapid Prototyping and Additive Manufacturing solutions using all major 3D printing systems including SLA Rapid Prototypes. Fast and Free online quotes at www.axisproto.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density  1.16 g/cc
@Temperature 25.0 °C
0.0419 lb/in³
@Temperature 77.0 °F
Liquid
 1.21 g/cc
@Temperature 25.0 °C
0.0437 lb/in³
@Temperature 77.0 °F
Solid
Viscosity 485 cP
@Temperature 30.0 °C
485 cP
@Temperature 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8686ASTM D2240
Tensile Strength, Yield 62.0 - 76.0 MPa8990 - 11000 psiASTM D638
Elongation at Break 3.1 - 5.6 %3.1 - 5.6 %ASTM D638
Tensile Modulus 3.048 - 3.532 GPa442.1 - 512.3 ksiASTM D638
Flexural Strength 89.0 - 115 MPa12900 - 16700 psiASTM D790
Flexural Modulus 2.827 - 3.186 GPa410.0 - 462.1 ksiASTM D790
Izod Impact, Notched 0.149 - 0.277 J/cm0.279 - 0.519 ft-lb/inASTM D256
Penetration 6.36.3mils; Viper/SLA 3500
 6.86.8mils; SLA 7000
 6.96.9mils; SLA 5000
 
Thermal PropertiesMetricEnglishComments
CTE, linear  64.0 µm/m-°C
@Temperature 0.000 - 20.0 °C
35.6 µin/in-°F
@Temperature 32.0 - 68.0 °F
T
 170 µm/m-°C
@Temperature 90.0 - 150 °C
94.4 µin/in-°F
@Temperature 194 - 302 °F
T>Tg; ASTM E831-93
Deflection Temperature at 0.46 MPa (66 psi) 58.0 °C136 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FASTM D648
Glass Transition Temp, Tg 62.0 °C144 °FDMA, E"
 
Descriptive Properties
AppearanceClear amber
Critical Exposure (mJ/cm²)13.8Viper/SLA 3500
 15.5SLA 7000
 17.7SLA 5000
Tested Build StylesFAST™, EXACT HR, QuickCast™ and ThinLayer™

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3D Systems Accura® Xtreme Plastic for SLA® Systems
Overview of materials for Polylactic Acid (PLA) Biopolymer
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
ALM D80-ST Nylon 11 SLS Prototyping Polymer
3D Systems Accura® Xtreme White 200 Plastic

PAPPR102 / 83481

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.