MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite Varcum 29153 Phenolic Resin
Categories: Polymer; Thermoset; Phenolic

Material Notes: Varcum 29153 is a one-step liquid phenolic resin in a mixture of butanol and diacetone alcohol.

APPLICATION: Baking-type, metal coating formulation.

FEATURES

  • A versatile, general purpose resin suitable for formulating coatings for a wide variety of applications.
  • Provides excellent resistance to solvents and acids.
  • Good alkali resistance.
  • Provides good flexibility of the cured film.
  • Excellent performance in baking coating formulations for metal surfaces requiring shaping of the metal after coating and curing.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 18000 cP
@Temperature 25.0 °C
DCT 4003F
 
Processing PropertiesOriginal ValueComments
Cure Time 100 sec
@Temperature 150 °C
DCT 4001A
 
Descriptive Properties
Non Volatile (%)68DCT 4005A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Phenolic; Unreinforced; Molded
Solvay MTM® 82S-C Phenolic Resin Matrix
Vitreous Carbon (Glassy Carbon)
Tipco Tipcolite® TPF 1115 - Unreinforced Thermoset Phenolic Resin, 43 mm Norton Flow with 9% Hexamine
Sumitomo Bakelite Durez® 175 Phenolic Resin

PSUMIT684 / 194489

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.