MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Exceed™ 1018LA Metallocene Polyethylene Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength properties, along with excellent drawability, allow downgauging in bag application.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: 4500 ppm
  • Slip: 450 ppm
  • Processing Aid: Yes
  • Thermal Stabilizer: Yes
Applications:
  • Agricultural Film
  • Bag in Box
  • Barrier Food Packaging
  • Blown Film
  • Bread Bags
  • Food packaging
  • Form Fill and Seal Packaging
  • Freezer Film
  • General Packaging
  • Heavy Duty Bags
  • Industrial Packaging
  • Lamination Film
  • Multilayer Packaging Film
  • Overwrap Film
  • Packaging Films
  • Premium Trash Bags
  • Stand Up Pouches
  • Trash Bags
  • Trash Can Liners

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccExxonMobil method
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Antiblock Level 4500 ppm
Slip Level 450 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 1400 psiASTM D882
Film Tensile Strength at Yield, TD 1400 psiASTM D882
Film Elongation at Break, MD 500 %ASTM D882
Film Elongation at Break, TD 600 %ASTM D882
Puncture Energy 16.0 in-lbExxonMobil Method
Elmendorf Tear Strength MD 250 gASTM D1922
Elmendorf Tear Strength TD 470 gASTM D1922
Dart Drop Test 460 gASTM D1709
Film Tensile Strength at Break, MD 7900 psiASTM D882
Film Tensile Strength at Break, TD 6200 psiASTM D882
1% Secant Modulus, MD 27000 psiASTM D882
1% Secant Modulus, TD 28000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 247 °FPeak Melting Point; ExxonMobil method
 
Optical PropertiesOriginal ValueComments
Haze 18 %ASTM D1003
Gloss 39 %45°; ASTM D2457
 
Descriptive Properties
Puncture Force8 lbfExxonMobil Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Exceed™ 2018EB Metallocene Polyethylene Resin (European Grade)
Dow Engage® 8400 Polyolefin Elastomer
ExxonMobil Exceed™ 3527PA Metallocene Polyethylene Resin (European Grade)
Dow Engage® 8003 Polyolefin Elastomer
ExxonMobil Exceed™ 1327CA Blown Film Resin

PEX99031 / 175267

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.