MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemours Krytox™ GPL 2E0 PFPE Grease
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE)

Material Notes: Krytox™ GPL 2E(x) lubricants are formulated using anti-rust additives more advanced than sodium nitrate. These additives are effective at low concentration levels, are environmentally friendly, and do not pose any restrictions on long-term recyclability of the grease. GPL Krytox™ GPL E series lubricants are high quality, ultrahigh performance anti-friction and anti-rust lubricants. Formulated with synthetic perfluoropolyether fluids, organic anti-rust additives, and efficient polytetrafluoroethylene (PTFE) thickeners.

Information provided by Chemours Krytox

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  1.87 g/cc
@Temperature 0.000 °C
0.0676 lb/in³
@Temperature 32.0 °F
oil
 1.87 g/cc
@Temperature 100 °C
0.0676 lb/in³
@Temperature 212 °F
oil
Viscosity Measure  4.0 cSt
@Temperature 40.0 °C
4.0 cSt
@Temperature 104 °F
oil
 7.0 cSt
@Temperature 20.0 °C
7.0 cSt
@Temperature 68.0 °F
oil
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 66.0 °C151 °F
Minimum Service Temperature, Air -70.0 °C-94.0 °F
Pour Point <= 70.0 °C<= 158 °Fbase oil
 
Descriptive Properties
ISO Grade of Base Oil5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WDUPJ841 / 254029

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.