MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Desmodur® E 2200/76 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Desmodur® E 2200/76 is a prepolymer based on diphenylmethane-diisocyanate (MDI) with isomers.

Properties / Applications: Desmodur® E 2200/76 is suitable for the flexibilization of Desmodur® E 21/E 23 or similar products, as a binder for granular rubber or in combination with suitable polyols for the formulation of flexible coatings and sealing compounds. Desmodur® E 2200/76 can also be used as a raw material for the formulation of solvent-free, moisture-curing, one-component adhesives or in combination with Baycoll® for the formulation of two-component adhesives. Such adhesives can be used to bond a wide variety of materials such as wood, metal and plastic. It must be ensured that the containers - including those that are empty – are kept sealed. Above all, contact with water must be prevented as it reacts with Desmodur® E 2200/76 to form polyureas and carbon dioxide. During storage, sample withdrawal, transfer and processing of Desmodur® E 2200/76, the ingress of water in any form (damp containers, aqueous solvents, moist air) must be prevented as otherwise the formation of carbon dioxide may cause a dangerous increase in pressure in the tanks and containers. Furthermore, the formation of polyureas in Desmodur® E 2200/76 may cause turbidity and possibly solid deposits which may then block filters, pumps and pipelines.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/ccDIN 51 757
Viscosity 2000 - 3500 cPMDI-01-02
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 200 °CDIN 51 758
 
Descriptive Properties
Content9.6-10.1%NCO, MDI-01-01

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Desmodur® E 1160 MPA/X Polyurethane
Covestro Desmodur® E 210 Polyurethane
Covestro Desmodur® E 21 Polyurethane
Covestro Desmodur® E 15 Polyurethane
Covestro Desmodur® E 23 A Polyurethane

PCOVEST0343 / 202126

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.