MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
TIMET TIMETAL® 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness, <3.00 in, Annealed, Per ASTM B348
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Beta Titanium Alloy

Material Notes: Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod or Thickness, <3.00 in, Annealed, Per ASTM B348; other specific form/thickness entries are also available in MatWeb.

Industry Specifications: USA Aerospace: AMS 4911, 4928, 4932, 4935, 4954, 4965, 4967. Germany Engineering: 3.7165. Germany Aerospace: 3.7164. France: T-A6V. UK Aerospace Specifications BS TA. 10,11, 12, 13, 28, 56 DTD 5363.

Features: A versatile medium strength alloy, the "workhorse" TIMETAL 6-4 exhibits good tensile properties at room temperature, creep resistance up to 325°C and excellent fatigue strength. It is often used in less critical applications up to 400°C. TIMETAL 6-4 is the alloy most commonly used in wrought and cast forms. Palladium or ruthenium can be added for increased corrosion resistance. Most properties are affected by the microstructure, which is determined by the thermomechanical history. It is highly resistant to general corrosion in sea water. This alloy is available in most common product forms including billet, bar, wire, plate, and sheet.

Data provided by TIMET.

Key Words: Ti-6-4; UNS R56400; ASTM Grade 5 titanium; Ti6Al4V, Ti64, Titanium 6-4
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 4.42 g/ccTypical
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate >= 895 MPaLongitudinal
 600 MPa
@Temperature 500 °C
Typical
 750 MPa
@Temperature 300 °C
Typical
 880 MPa
@Temperature 100 °C
Typical
Tensile Strength, Yield >= 828 MPa
@Strain 0.2 %
Longitudinal
 460 MPa
@Strain 0.2 %,
Temperature 500 °C
Typical
 625 MPa
@Strain 0.2 %,
Temperature 300 °C
Typical
 800 MPa
@Strain 0.2 %,
Temperature 100 °C
Typical
Elongation at Break >= 10 %Longitudinal
Reduction of Area >= 25 %Longitudinal
Modulus of Elasticity 95.0 - 111 GPa
@Temperature 230 °C
varies with heat treatment and texture
 107 - 122 GPa
@Temperature 20.0 °C
varies with heat treatment and texture
Poissons Ratio 0.31
Shear Modulus 41.0 - 45.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000168 ohm-cm
 0.000168 ohm-cm
@Temperature 0.000 °C
 0.000186 ohm-cm
@Temperature 315 °C
 0.000189 ohm-cm
@Temperature 650 °C
Magnetic Permeability 1.00005at 20 Oersted
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.00 µm/m-°C
@Temperature 0.000 - 100 °C
 9.40 µm/m-°C
@Temperature 20.0 - 425 °C
 9.70 µm/m-°C
@Temperature 20.0 - 650 °C
Specific Heat Capacity 0.580 J/g-°C
@Temperature 20.0 °C
 0.670 J/g-°C
@Temperature 425 °C
 0.930 J/g-°C
@Temperature 870 °C
Thermal Conductivity 6.60 W/m-K
@Temperature 20.0 °C
 10.6 W/m-K
@Temperature 315 °C
 17.5 W/m-K
@Temperature 650 °C
Melting Point <= 1660 °C
Liquidus >= 1636 °C
 1660 °C
Maximum Service Temperature, Air 350 °CReasonable mechanical properties retained
Beta Transus 995 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 5.5 - 6.75 %
Carbon, C <= 0.080 %
Hydrogen, H <= 0.015 %
Iron, Fe <= 0.40 %
Nitrogen, N <= 0.050 %
Other, each <= 0.10 %
Other, total <= 0.40 %
Oxygen, O <= 0.20 %
Titanium, Ti 87.6 - 91 %Calculated as remainder
Vanadium, V 3.5 - 4.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Ti-6Al-4V (Grade 5), Annealed
Titanium Ti-6Al-4V ELI (Grade 23), Annealed
Titanium Ti-6Al-4V (Grade 5), STA
TIMET TIMETAL® 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; 1.75 - 2.50 in Rod or Thickness; Per ASTM F136)

NTIME64D / 19324

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.