MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil 20W-50 Exxon Aviation Oil
Categories: Fluid; Lubricant

Material Notes: Aviation Oil 100, 120 and 20W-50 are  non-dispersant, mineral oil-based lubricants for piston engines of commercial, military and private aircraft. They contain very low concentrations of anti-oxidant, anti-foam and pour point depressant. Aviation Oil 100 and 120 are monogrades of SAE 50 and SAE 60 grade, correspondingly. Aviation Oil 20W-50 is a multi-grade lubricant. High manufacturing standards ensure the dependability of Aviation Oil under the exacting conditions of modern piston engine service. They are approved by leading engine manufacturers throughout the world.

Despite the advent and wide-spread use of ashless-dispersant aviation engine oils, some operators prefer to continue the use of non-dispersant mineral oil lubricants, which have provided excellent service for many years. In addition, many engine builders and overhaul agencies recommend or require the use of non-dispersant oils for break-in of new or newly overhauled engines. Aviation Oil of a viscosity grade selected to match the ambient temperature operation conditions of the aircraft meets these needs in accordance with the requirements of all major engine manufacturers. Aviation Oil products are U.S. Military approved under SAE J1966, which replaced MIL-L-6082E and are listed in the U.S. Military Qualified Products List QPL-1966. Specific viscosity grades are approved by Pratt and Whitney, Teledyne Continental Motors, and Textron Lycoming, and are included in their qualified products lists.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.882 g/cc
@Temperature 15.6 °C
ASTM D4052
API Gravity 28.9 °
Viscosity 5.1 cP
@Temperature 150 °C
High Temperature High Shear (HTHS); ASTM D4683
 6900 cP
@Temperature -15.0 °C
Cold Cranking Simulator (CCS); ASTM D5293
Viscosity Measurement 132Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 179 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 20.3 cStASTM D445
Ash 0.00 %SAE J1747
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.020mgKOH/g; ASTM D664
 
Thermal PropertiesOriginal ValueComments
Pour Point -24.0 °CASTM D97
Flash Point 240 °CASTM D92
 
Component Elements PropertiesOriginal ValueComments
Sulfur, S 0.40 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil 20W-50 Exxon Aviation Oil Elite

WEXXON360 / 75785

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.