MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Cosmic Plastics FARBOSET® 1190 Black Mineral and Glass Filled Epoxy Molding Compound
Categories: Polymer; Thermoset; Epoxy; Epoxy, Molded, Glass Fiber Filler; Epoxy, Molded, Mineral Filled

Material Notes: Cosmic FARBOSET 1190 Black is a fast curing, mineral & glass filled, epoxy molding compound with improved strength properties. It is designed for the encapsulation of coils, transformers, switches and other electrical and electronic components requiring excellent thermal shock resistance. This material exhibits superior resistance to cracking.

Information provided by Cosmic Plastics Inc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 1.00 g/ccpowder
Density 1.91 g/cc
Linear Mold Shrinkage 0.0050 in/in
Spiral Flow 69.0 cmEMMI 1-66A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85
Tensile Strength at Break 14000 psi
Flexural Strength 20000 psi
Compressive Strength 35000 psi
Izod Impact, Notched 0.600 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cm
Surface Resistance 1.00e+16 ohm
Dielectric Constant 3.8
@Frequency 1000 Hz
Dielectric Strength 350 V/milshort time 125 mil
Dissipation Factor 0.0040
@Frequency 1000 Hz
Dielectric Loss Index 0.015
@Frequency 1000 Hz
Arc Resistance 200 sec
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.00200 cal cm/sec-cm²-°C
Maximum Service Temperature, Air 200 °C
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
 
Processing PropertiesOriginal ValueComments
Mold Temperature 150 - 180 °C
Cure Time 1.50 - 3.00 min
@Temperature 150 °C
 42.0 sec
@Temperature 150 °C
Hot Plate
Shelf Life 0.0670 Month
@Temperature 35.0 °C
2 days
 0.250 Month
@Temperature 25.0 °C
1 week
 12.0 Month
@Temperature 5.00 °C
 
Descriptive Properties
Molding Pressure50-1000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hippe EP GC 205 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Hippe EP GC 204 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Hippe EP GC 203 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Hippe EP GC 202 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Hippe EP GC 201 Woven Glass Cloth Reinforced Epoxy Resin - Sheet

PCOSM027 / 190809

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.