MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Potters Industries Q-Cel® 5023  (discontinued **)
Categories: Ceramic; Glass; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Q-CEL® products offer formulators flexibility in polymer composites. The addition of hollow spheres to fiberglass reinforced plastics (FRP), epoxy, compounds, and urethane castings can provide weight reduction cost savings and improved impact resistance. Insulating features of hollow spheres also work to the chemists’ advantage in thermal shock and heat transfer areas. They are suited for many applications, including fiberglass reinforced plastics, urethane foams, putties, cultured marble and adhesives.

Information provided by Potters Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.130 g/cc
Density 0.230 g/ccEffective density of spheres
Particle Size 5.0 - 130 µmrange
 70 µmmean value
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 500 psiMaximum working pressure

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Potters Industries Q-Cel® 5028
Fibre Glast 180 Clear Gel Coat
DuPont Mobility and Materials Vespel® CR-6100 Carbon-Reinforced Fluoropolymer
SPHERE ONE EXTENDOSPHERES™ XOL-150 Hollow Spheres
ICO Polymers ICOFLO™ 510-5023 400 Micron LDPE Powder

CPOT19 / 1757

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.