MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Durethan® DP 2801 000000 Nylon 66 (PA66), Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: PA 66 injection molding grade, non-reinforced, UL 94V-2 off 0,75 mm (listed), GWFI: 960°C off 0.75 mm, GWIT: 775°C off 0,75 mm, halogen-free

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.143 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0114 cm/cm60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0122 cm/cm60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Puncture Resistance 3730 N
@Temperature 23.0 °C
ISO 6603-2
 4630 N
@Temperature -30.0 °C
ISO 6603-2
Ball Indentation Hardness 151 MPaISO 2093-1
Tensile Strength at Break 80.0 MPa5 mm/min; ISO 527-1,-2
Tensile Strength, Yield 94.0 MPa50 mm/min; ISO 527-1,-2
Elongation at Break 10 %Nominal, 50 mm/min; ISO 527-1,-2
 11 %5 mm/min; ISO 527-1,-2
Elongation at Yield 4.2 %50 mm/min; ISO 527-1,-2
Tensile Modulus 3500 MPa1 mm/min; ISO 527-1,-2
Flexural Strength 127 MPa2 mm/min; ISO 178-A
Flexural Yield Strength 105 MPa
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 3200 MPa2 mm/min; ISO 178-A
Flexural Strain at Break 6.2 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) <= 10.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1A
 <= 10.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1A
Izod Impact, Unnotched (ISO) 80.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1U
 110 kJ/m²
@Temperature -30.0 °C
ISO 180-1U
Charpy Impact Unnotched 110 kJ/m²
@Temperature 23.0 °C
ISO 179-1eU
 120 kJ/m²
@Temperature -30.0 °C
ISO 179-1eU
Charpy Impact, Notched <= 10.0 kJ/m²
@Temperature 23.0 °C
ISO 179 1eA
 <= 10.0 kJ/m²
@Temperature -30.0 °C
ISO 179 1eA
Puncture Energy 5.10 J
@Temperature -30.0 °C
ISO 6603-2
 13.1 J
@Temperature 23.0 °C
ISO 6603-2
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 400 VSolution B; IEC 60112
 600 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Melting Point 265 °C10°C/min; ISO 11357-1,-3
Maximum Service Temperature, Air 249 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 210 °CISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °CISO 75-1,-2
Deflection Temperature at 8.0 MPa 60.0 °CISO 75-1,-2
Vicat Softening Point >= 230 °C
@Load 5.10 kg
120°C/h; ISO 306
Flammability, UL94 V-2
@Thickness 0.750 mm
Oxygen Index 30 %Method A; ISO 4589-2
Glow Wire Ignition Temperature 775 °C
@Thickness 0.750 mm
IEC 60695-2-13
 775 °C
@Thickness 1.50 mm
IEC 60695-2-13
 775 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
Shrinkage, MD 0.42 %
@Treatment Temp. 120 °C,
Time 14400 sec
Post-Shrinkage Flow Direction; 60x60x2; ISO 294-4
Shrinkage, TD 0.11 %
@Treatment Temp. 120 °C,
Time 14400 sec
60x60x2; ISO 294-4
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 °Cinjection molding
 260 - 270 °C
Mold Temperature 80.0 °Cinjection molding
 80.0 - 100 °C
Drying Temperature 80.0 °C
Dry Time 2.00 - 6.00 hour
Moisture Content 0.030 - 0.070 %Karl Fischer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® 1310-11 NF2001 PA66 (Dry)
Celanese CoolPoly® D3612 Thermally Conductive Polyamide (PA66/6)
BASF Ultramid® 1000-11 NF2001 PA66 (Dry)
Asahi Kasei Thermylon® N3-25FG-2726 PA66-GF25
EMS-Grivory Grilon® AG-25 HM PA66-GF25

PLANW9480 / 208335

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.