MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Samyang Triel® 5350 Thermoplastics Polyetherester Elastomer, General Extrusion
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester, TP; Polyether Ester Elastomer

Material Notes: Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.
5350 is an extrusion grade.

Applications: Elastic thread

Information provided by Samyang.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/ccASTM D792
Water Absorption 0.50 %ASTM D570
Linear Mold Shrinkage 0.015 - 0.017 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 35ASTM D2240
Tensile Strength, Ultimate 150 kg(f)/cm²ASTM D638
Tensile Stress at Strain 45.0 kg(f)/cm²
@Strain 5.0 %
ASTM D638
 60.0 kg(f)/cm²
@Strain 10 %
ASTM D638
 85.0 kg(f)/cm²
@Strain 50 %
ASTM D638
Izod Impact, Notched NB
@Thickness 3.17 mm,
Temperature -40.0 °C
ASTM D256
 NB
@Thickness 3.17 mm,
Temperature 23.0 °C
ASTM D256
 
Descriptive Properties
Flexible Rate> 400%ASTM D638

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Samyang Triel® 5700 Thermoplastics Polyetherester Elastomer, General Extrusion
Samyang Triel® 5401BM Thermoplastics Polyetherester Elastomer, Blow Molding
Samyang Triel® 5400 Thermoplastic Polyether Ester Elastomer
Samyang Triel® 5302FR Thermoplastics Polyetherester Elastomer, Non-Halogen Flame Retardancy
Samyang Triel® 5301SP Thermoplastics Polyetherester Elastomer, Double Extrusion

PSANX943 / 133337

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.