MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Solaxis ASA 3D Printing Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; ASA Polymer

Material Notes: Used to build consistently high-quality parts, with exceptional UV stability and the best aesthetics of any FDM® thermoplastic. ASA is a popular all-purpose prototyping material for users of Fortus 380mc™, 450mc™ and 900mc™ 3D Printers, and the Stratasys F123 ™ Series. ASA parts can match or exceed the mechanical properties of ABS in general prototyping uses. Its UV-resistance makes it especially suited to production parts for outdoor commercial and infrastructure use. Its wide selection of colors and matte finish makes it ideal for attractive prototypes in consumer sporting goods, tools and automotive components and accessories.

Information provided by Solaxis Ingenious Manufacturing

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 82ASTM D785
Tensile Strength, Ultimate 30.0 MPa
@Thickness 3.17 mm
ZX Orientation, Type 1, 0.2 in./min; ASTM D638
 33.0 MPa
@Thickness 3.17 mm
XZ Orientation, Type 1, 0.2 in./min; ASTM D638
Tensile Strength, Yield 27.0 MPa
@Thickness 3.17 mm
ZX Orientation, Type 1, 0.2 in./min; ASTM D638
 29.0 MPa
@Thickness 3.17 mm
XZ Orientation, Type 1, 0.2 in./min; ASTM D638
Elongation at Break 3.0 %
@Thickness 3.17 mm
ZX Orientation, Type 1, 0.2 in./min; ASTM D638
 9.0 %
@Thickness 3.17 mm
XZ Orientation, Type 1, 0.2 in./min; ASTM D638
Elongation at Yield 2.0 %
@Thickness 3.17 mm
XZ Orientation, Type 1, 0.2 in./min; ASTM D638
 2.0 %
@Thickness 3.17 mm
ZX Orientation, Type 1, 0.2 in./min; ASTM D638
Tensile Modulus 1.95 GPa
@Thickness 3.17 mm
ZX Orientation, Type 1, 0.2 in./min; ASTM D638
 2.01 GPa
@Thickness 3.17 mm
XZ Orientation, Type 1, 0.2 in./min; ASTM D638
Flexural Strength 48.0 MPaZX Orientation, Method 1, 0.05 in./min; ASTM D790
 60.0 MPaXZ Orientation, Method 1, 0.05 in./min; ASTM D790
Flexural Modulus 1.63 GPaZX Orientation, Method 1, 0.05 in./min; ASTM D790
 1.87 GPaXZ Orientation, Method 1, 0.05 in./min; ASTM D790
Flexural Strain at Break 4.0 %ZX Orientation, Method 1, 0.05 in./min; ASTM D790
Izod Impact, Notched 64.0 J/mXZ orientation, Method A; ASTM D256
Izod Impact, Unnotched 321 J/mXZ orientation, Method A; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 - 1.00e+15 ohm-cmXZ; ASTM D257
Dielectric Constant 2.97 - 3.04XZ; ASTM D150-98
Dielectric Strength 329 V/milXZ; ASTM D149-09, Method A
 414 V/milZX; ASTM D149-09, Method A
Dissipation Factor 0.0090XZ; ASTM D150-98
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 8.79 µm/m-°CASTM E831
CTE, linear, Transverse to Flow 8.28 µm/m-°CASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °CASTM D648
Vicat Softening Point 103 °CRate B/50; ASTM D1525
Glass Transition Temp, Tg 108 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOLXIS982 / 256139

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.