MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Abatron KromaKote 8901-8 Polyurethane Coating  (discontinued **)
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: 2-component system for outstanding performance in normal, industrial, marine and corrosive environments. Superb combination of chemical, solvent, abrasion and weather resistance.

Suggested Uses: Protective and decorative coating and resurfacing of tanks, tubs, sinks, tiles, appliances, metal panels, machinery, bulkheads, walls, counters, and all kinds of indoor and outdoor surfaces.

Available in custom colors.

Processing: Ratio by volume: 2 parts Kromakote 8901-8 Part A (colored resin solution) to 1 part Kromakote 8901-8 Part B (clear coreactant solution).

Information provided by Abatron.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 10.6 lb/gal11.6# part A, 8.8# part B
Solids Content 67.8 %By weight
Volatile Organic Compounds (VOC) Content 412 g/l
Viscosity 300 cPApproximately
 
Mechanical PropertiesOriginal ValueComments
Taber Abrasion, mg/1000 Cycles 18CS-17 wheel, 1000 gm load
 
Processing PropertiesOriginal ValueComments
Pot Life 120 - 240 min
 
Descriptive Properties
Pencil Hardness3H

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SGL Carbon Group SIGRAFIL C® C25 S003 PUT Staple Carbon Fiber, Polyurethane Sizing
Overview of materials for ABS/Polyurethane Alloy
Overview of materials for Thermoset Polyurethane, Liquid
Abatron AboThane 8003-3 Polyurethane Coating
AorTech Biomaterials Elast-Eon™ E2A Biomedical Polyurethane Pellets

PABKW003 / 22044

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.