MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman Premi-Glas® 2550® AM CR-SX Fiberglass Reinforced Thermoset SMC
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset

Material Notes: Premi-Glas 2550® AM CR-SX is an advanced fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications where stringent flame spread and smoke generation criteria are required in combination with anti-microbial properties.

Key features and benefits are:

  • Non-Halogen FR technology, and proprietary Anti-Microbial agents
  • Meets Steiner Tunnel < 25 Flame spread index and < 50 Smoke index
  • Required in some instances where > 10 square feet of composite is present
  • Suitable for outdoor use in applications involving UV exposure and water immersion in accordance with UL746C (f1), file E42524
  • Designed for compression molding in matched metal die molds.

A. Schulman has acquired this former Premix product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.00 g/cc2.00 g/cc
Linear Mold Shrinkage 0.00025 cm/cm0.00025 in/inPolymerization Shrinkage
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 58.0 MPa8410 psiASTM D638
Tensile Modulus 12.0 GPa1740 ksiASTM D638
Flexural Strength 135 MPa19600 psiASTM D790
Flexural Modulus 11.0 GPa1600 ksiASTM D790
Izod Impact, Notched 5.10 J/cm9.55 ft-lb/inASTM D256
Izod Impact, Unnotched 7.70 J/cm14.4 ft-lb/inASTM D4812
 
Thermal PropertiesMetricEnglishComments
UL RTI, Electrical 130 °C266 °FUL 746C
UL RTI, Mechanical with Impact 130 °C266 °FUL 746C
UL RTI, Mechanical without Impact 130 °C266 °FUL 746C
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 5VB
@Thickness 1.50 mm
5VB
@Thickness 0.0591 in
Flame Spread Index 1010UL723 Steiner Tunnel
 
Processing PropertiesMetricEnglishComments
Processing Temperature 150 °C302 °FCompression Molding
Clamp Pressure 3.45 - 6.89 MPa500 - 1000 psiMolding Pressure
 
Descriptive Properties
Smoke Developed Index40UL723 Steiner Tunnel

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Premi-Glas® 1200H-22 Fiberglass Reinforced Thermoset SMC
Aluminum 6063-T6
ASTM A542 Low Alloy Steel, Grade A, Class 4
AISI 4140 Steel, annealed at 815°C (1500°F) furnace cooled 11°C (20°F)/hour to 665°C (1230°F), air cooled, 25 mm (1 in.) round
AISI 5160 Steel, oil quenched from 830°C (1525°F), 650°C (1200°F) temper, 25 mm (1 in.) round

PPREMH969 / 140367

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.