MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ LUBRICOMP™ Compound DL004 Polycarbonate (PC) (Europe)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP LUBRICOMP DL004 compound is based on Polycarbonate (PC) resin containing 20% PTFE. Added features of this grade include: Wear Resistant.

Features: Wear resistant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.32 g/cc0.0477 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 47.0 MPa6820 psi5 mm/min; ISO 527
Elongation at Yield 5.3 %5.3 %5 mm/min; ISO 527
Tensile Modulus 2.10 GPa305 ksi1 mm/min; ISO 527
Flexural Strength 77.0 MPa11200 psiyield, 2 mm/min; ISO 178
Flexural Modulus 2.10 GPa305 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO) 17.0 kJ/m²8.09 ft-lb/in²80*10*4; ISO 180/1A
Coefficient of Friction, Dynamic 0.250.25ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.210.21ASTM D3702 Modified: Manual
K (wear) Factor 62.4 x 10-8 mm³/N-M31.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 79.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
43.9 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 79.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
43.9 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 139 °C282 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 127 °C261 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94  HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
UL 94
 V-1
@Thickness >=3.00 mm
V-1
@Thickness >=0.118 in
UL 94
 
Processing PropertiesMetricEnglishComments
Zone 2 305 - 315 °C581 - 599 °F
Zone 3 310 - 320 °C590 - 608 °F
Melt Temperature 300 - 315 °C572 - 599 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80746 / 288693

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.