MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Park Aerospace Nelcote® F-554 Phenolic Prepreg, Aerospace Silica Fabric Reinforced
Categories: Polymer; Thermoset; Phenolic

Material Notes: Nelcote® F-554 is a high purity silica filled phenolic resin coated on Commercial or Aerospace grade silica fabric. F-554 is used in the manufacture of intermediate temperature ablative rocket nozzles, heat shields, and combustion chambers in highly oxidative environments.

Key Features and Benefits:

  • Provides a combination of high-strength and ablative properties for demanding applications
  • Low thermal expansion
  • Good Tack and Drape properties
  • Conforms to MIL-R-9299

Applications/Qualifications:

  • Rocket Nozzles
  • Combustion Chambers
  • Heat Shields
  • Rocket Motor Throat Sections

Information provided by Park Electrochemical Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.70 g/ccASTM D792
Filler Content 2.0 - 4.0 %
Volatiles 2.0 - 5.0 %
@Temperature 163 °C
10 min
Thickness 21.0 milnominal, cured, per ply
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 70ASTM D2583
Tensile Strength, Yield 13000 psi
@Temperature 23.9 °C
0° Direction, Dry; 325°F Autoclave; ASTM D638
Tensile Modulus 2400 ksi
@Temperature 23.9 °C
0° Direction, Dry; 325°F Autoclave; ASTM D638
Flexural Strength 23.0 ksi
@Temperature 23.9 °C
Dry; 325°F Autoclave; ASTM D790
Flexural Modulus 2500 ksi
@Temperature 23.9 °C
Dry; 325°F Autoclave; ASTM D790
Compressive Strength 24.0 ksi
@Temperature 23.9 °C
Dry; 325°F Autoclave; ASTM D695
Compressive Modulus 2400 ksi
@Temperature 23.9 °C
Dry; 325°F Autoclave; ASTM D695
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.240 BTU/lb-°FASTM C351
Thermal Conductivity 32.4 BTU-in/hr-ft²-°F
@Temperature 149 °C
ASTM C177
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature 4.44 °C
 
Descriptive Properties
Nominal Prepreg Weight (oz/yd)30
Resin Flow (%)7-17325°F, 150psi
Resin Solids Content (%)30-36

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Park Aerospace Nelcote® F-502 Phenolic Prepreg, Silica Reinforced
Park Aerospace Nelcote® F-557 Phenolic Prepreg, Aerospace Silica Fabric Reinforced
Park Aerospace Nelcote® F-557 Phenolic Prepreg, Commercial Silica Fabric Reinforced
Park Aerospace Nelcote® F-554 Phenolic Prepreg, Commercial Silica Fabric Reinforced
Park Aerospace Nelcote® F-562 Phenolic Prepreg, 8HS Silica Reinforced

PPARK052 / 89324

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.