MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco Cerama-Dip™ 538-N High Temperature Specialty Ceramic-Inorganic Coating  (discontinued **)
Categories: Ceramic; Oxide; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available.

Key Words: High Temperature Coatings
Vendors: Aremco’s high temperature coatings and sealers are formulated using ceramic, glass and silicone technologies for a broad range of electrical insulation applications. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.73 g/cc
Solids Content 41.7 %by volume
 64.6 %by weight
Volatile Organic Compounds (VOC) Content 0.00 g/l
Viscosity 2000 - 2500 cPBrooksfield LV Viscometer
Thickness 1.00 milrecommended dry film thickness
 2.40 milestimated wet film thickness
Storage Temperature 55.0 - 85.0 °F
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 135 V/mil
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 2600 °FContinuous
 
Processing PropertiesOriginal ValueComments
Dry Time 1 hourTouch
 1 hourHandling
Cure Time >= 1.00 hourAir Set prior to curing
 3.00 - 6.00 hour2-4 hr at 200°F followed by 1-2 hr at 350°F
Shelf Life 6.0 Month
@Temperature 12.8 - 29.4 °C
 
Descriptive Properties
Application Temperature50 - 90°F
ColorLight Gray
Dry Film Coverage ft2/gal668at 1 mil
Thinner538-N-T

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LATI Larpeek 10 G/60 PEEK, 60% Glass Fiber Reinforced
Aremco Cerama-Dip™ 538-N-GRN High Temperature Specialty Ceramic-Inorganic Coating
Aremco Cerama-Dip™ 538-N-BLK High Temperature Specialty Ceramic-Inorganic Coating
LATI Laticonther 88/10 GR/50 PEEK, 50% Graphite Reinforced
Aremco Ceramacoat™ 845-WHT High Temperature Ceramic-Inorganic Coating

ZCAREM39 / 580

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.