MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BYK Mineral Colloid® BP Bentonite
Categories: Ceramic; Clay

Material Notes: Description: Mineral Colloid BP is a high purity montmorillonite refined from carefully selected natural bentonite. The unique characteristics, consistent properties and high purity are made possible by our statistically controlled processing.

Uses and Advantages:

  • Mineral Colloid BP exhibits excellent thixotropic properties , enhancing suspension, stability and viscosity control
  • The use of Mineral Colloid BP increases sag resistance and reduces syneresis and settling.
  • Mineral Colloid BP is totally inorganic and therefore not susceptible to enzyme attack.
  • Mineral Colloid BP is not affected by high shear or high temperatures during manufacturing. Mineral Colloid BP can be sheared repeatedly.
  • The type of rheology Mineral Colloid BP exhibits lends itself to excellent spray atomization.
  • Low levels of Mineral Colloid BP are needed in a paint system because of its high gel strength.

    Information provided by Southern Clay Products

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Brookfield Viscosity 4450 cP4450 cP100 rpm
     29800 cP29800 cP10 rpm
     166000 cP166000 cP1 rpm
     
    Descriptive Properties
    Leneta22 SAG
    Stormer114 KU
    Syneresis<1%10 days at 120°F

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    BYK Nanothix® B1490 Phylosilicate
    BYK Necowel FLE 55N Clay Additive
    BYK Mineral Colloid® MO Clay Additive
    BYK Laponite® XLS Synthetic Layered Silicate
    BYK Laponite® XLG Synthetic Layered Silicate

    PBYK073 / 185070

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.