MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Borcell™ HE1102 High Density Polyethylene Compound for Gas Injection of Cellular Communication Cable Insulation  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Borcell HE1102 is a high density polyethylene. A nucleating agent is incorporated for a uniform and closed cell structure. The components in the formulation are selected to give the lowest possible dielectric loss.

Borcell HE1102 HDPE is intended for the insulation of communication cables using a gas-injection foaming process. Borcell HE1102 is suitable for thick walled coax cables, minicoax cables and telephone signals. With proper processing conditions it is possible to produce coax cables with an expansion degree of 75%.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.948 g/ccASTM D792
Melt Flow 0.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 61ASTM D2240
Tensile Strength, Yield 3600 psiASTM D638
Elongation at Break 200 %ASTM D638
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.35
@Frequency 1e+6 Hz
ASTM D1531
Dielectric Strength >= 700 V/milAt 20 mils; ASTM D3755
Dissipation Factor 0.000050
@Frequency 1e+6 Hz
ASTM D1531
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -76.0 °CASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis LE1120 Low Density Polyethylene for Physically Foamed Cellular Insulation
Borealis HE1344 High Density Polyethylene Compound for Cellular Insulation of Data Cables
Borealis HE1345 High Density Polyethylene Compound for Cellular Insulation of Telephone Singles
Borealis BS4641 High Density Polyethylene
Borealis BL2571 High Density Polyethylene

PBOREA026 / 27333

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.