MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Beijing Evergrow Resources UHMW PE Powder
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: Ultra-high molecular weight polyethylene (UHMWPE) is an outstanding engineering plastic. It’s characterized by the following properties.
    Features:
  • Very high abrasion resistance
  • Very high impact strength
  • Very low coefficient friction
  • Good self-lubricant
  • Excellent resistance to chemicals
  • Good resistance to low temperature
  • Excellent dielectric properties

Information provided by Beijing Evergrow Resources.

Key Words: UHMWPE, PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.450 g/cc
Density 0.935 g/cc
Volatiles <= 0.15 %Moisture
Particle Mesh Size 20 Mesh1% retained
Molecular Weight 3.00e+6 - 4.00e+6 g/mol
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 35.0 MPa
@Temperature 32.0 °C
Elongation at Break 200 - 300 %
Izod Impact, Unnotched NB
Izod Impact, Notched (ISO) >= 70.0 kJ/m²
 
Thermal PropertiesOriginal ValueComments
Heat Distortion Temperature >= 80.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Low Density Polyethylene (LDPE), Molded
Overview of materials for Medium Density Polyethylene (MDPE), Molded
Beijing Evergrow Resources UHF-R2400 UHMW PE Fiber
Polikim ULPOLEN® 1000 UHMWPE Standard
Westlake Plastics Lennite® Biocompatible Implant Grade UHMW-PE

PBEIJ001 / 90070

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.