MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Alathon 9305TC High Denisty Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Alathon high density polyethylene resins are produced in North America using slurry and solution technologies and include bi-modal HMW grades commonly used in pressure pipe and blown film, general purpose and thin-wall injection molding grades, and blown film grades known for their moisture barrier performance.

Alathon 9305TC is a high molecular weight high density copolymer with a broad bimodal molecular weight distribution. This resin exhibits high density, stiffness and good process ability. Typical applications for wire and cable include cable in conduit.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.949 g/cc0.0343 lb/in³ASTM D1505
ESCR 10% Igepal® >= 2000 hour>= 2000 hourCond. B; ASTM D1693
Thermal Stress Crack Resistance >= 2500 hour>= 2500 hourASTM D2951
Melt Flow 0.075 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.075 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ASTM D2240
Tensile Strength at Break 36.6 MPa5310 psiASTM D638
Tensile Strength, Yield 23.4 MPa3390 psiASTM D638
Elongation at Break 800 %800 %ASTM D638
Flexural Modulus, 1% Secant 1000 MPa145000 psiASTM D790
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.60e+17 ohm-cm2.60e+17 ohm-cmASTM D257
Dielectric Constant 2.33
@Frequency 1e+6 Hz
2.33
@Frequency 1e+6 Hz
ASTM D150
Dissipation Factor 0.000070
@Frequency 1e+6 Hz
0.000070
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 125 °C257 °FASTM D1525
Brittleness Temperature <= -76.0 °C<= -105 °FASTM D746
 
Descriptive Properties
Processing MethodWire & Cable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Petrothene LR52800E HDPE
LyondellBasell Petrothene® LR590001 High Density Polyethylene
LyondellBasell Alathon® L4904 High Density Polyethylene, Pipe and Sheet Extrusion Grade
LyondellBasell Alathon® L5008 High Density Polyethylene
LyondellBasell Alathon® L5008HP High Density Polyethylene, Pressure Pipe Extrusion Grade

PEQT7057 / 218695

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.