MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

1,2,4-Trimethylbenzene (Pseudocumene), C9H12
Categories: Fluid; Solvent

Key Words: C9H12
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.880 g/cc
@Temperature 20.0 °C
0.0318 lb/in³
@Temperature 68.0 °F
Viscosity 1.112 cP
@Temperature 20.0 °C
1.112 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 120.195 g/mol120.195 g/mol
Vapor Pressure 0.001929 bar
@Temperature 20.0 °C
1.447 torr
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 32.3 bar24200 torr
Critical Temperature 376 °C709 °F
Critical Density 0.280 g/cc0.0101 lb/in³
Critical Molar Volume 430 cm³/mol26.2 in³/mol
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 326.5 J/g140.5 BTU/lb
Specific Heat Capacity 1.281 J/g-°C
@Temperature 25.0 °C
0.3062 BTU/lb-°F
@Temperature 77.0 °F
Vapor
Thermal Conductivity 0.130 W/m-K
@Temperature 20.0 °C
0.902 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point -46.2 °C-51.2 °F
Boiling Point 169.4 °C336.9 °F
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter16.219
Antoine's Vapor Pressure B Parameter3622.58
Antoine's Vapor Pressure C Parameter-64.59
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)95-63-6
Chemical FormulaC9H12
Critical Compressibility (Zc)0.258
Dipole moment (p/C.m)1.001E-28
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A872.74
Dynamic Viscosity Parameter B297.75
Molar Heat Capacity (298K)153.911 J/mol-K
Molar Heat Capacity of Vapor a Parameter-4.6652
Molar Heat Capacity of Vapor b Parameter0.6234
Molar Heat Capacity of Vapor c Parameter-0.0003261
Molar Heat Capacity of Vapor d Parameter6.372E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

VORGS364 / 99711

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.