MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik ADOGEN® 66 Antistatic agent
Categories: Other Engineering Material

Material Notes: Composition: ADOGEN® 66 is 100 % Ethyl bis-(polyethoxyethanol) tallow ammonium ethosulfate.Application field:
  • ADOGEN® 66 quat is most commonly used as an antistatic agent, effective on cellulosic and synthetic fibers and fabrics
  • Water soluble, cationic surfactant, suggesting uses as a dispersing agent, dye retarder, and general purpose emulsifier.
  • Application rates at levels of 0.05 % -0.1 % based on fiber or fabric weight give demonstrable reductions in static charges.
Benefits:
  • Effective antistatic agent on polyester, nylon and acrylic fabrics
  • Very good thermal stability
  • Highly hydrophilic quaternary ammonium compound
  • Viscous liquid, free of solvents, non chloride salt
  • Non corrosive
  • Compatible with anionic

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 100 %
pH 7.010% IPA/water
Viscosity 300 - 500 cP
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 100 °CPensky-Martens CC
 
Optical PropertiesOriginal ValueComments
Gardner Color Number 6.0 - 8.0
 
Descriptive Properties
AppearanceViscous liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik BREAK-THRU® DA 646 Surfactants
Evonik ADOGEN® 66 Liquid
Evonik REWPAL® EO 70 Preparation agent
Evonik BREAK-THRU® DA 752 W Surfactants
Evonik BREAK-THRU® DA 675 Surfactants

PEVONIL674 / 196878

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.