MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubriplate SYN-H1-220 Polyalkylene Glycol-Based Synthetic Food Machinery Grade Fluid
Categories: Fluid; Lubricant; Polyglycol

Material Notes: Specifically designed for use where elevated temperatures exist and the need for a food grade lubricant is required. For chain applications where air temperatures exceed 400°F and up to 600°F when not exposed to open flame or ignition source. Passes 12 stages of FZG test.

SYN-H1-220 Fluid is available in Pails & Drums.

H-1 Class Lubricants are manufactured with ingredients that comply with FDA regulation 21 CFR 178.3570 for lubricants with incidental contact with the edible product.

Information provided by Lubriplate

Key Words: Part Number L0779-
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 206Viscosity Index
 220ISO Grade
Saybolt Viscosity at 100°F 1310 SUS
Saybolt Viscosity at 210°F 188 SUS
Kinematic Viscosity at 40°C (104°F) 285 cSt
Kinematic Viscosity at 100°C (212°F) 41 cSt
 
Thermal PropertiesOriginal ValueComments
Pour Point -20.0 °F
Flammability Test 550[°F] Fire Point
Flash Point 540 °F
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
SAE Gear Oil No.90

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WLUBR147 / 76193

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.