MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LATI LATAMID 66 H2 GK/30 30% Mixed Glass/Carbon Fiber, Heat-Stabilized Nylon 66  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass/Carbon Fiber Filled

Material Notes: Description: Latamid 66 is a family of Nylon 66 with various reinforcements and corresponding properties. They are distinguished by their excellent flowability, moldability and good mechanical and electrical properties. Glossy finish is achievable in a wide range of colors. Pieces made of Latamid 66 can be painted without any particular problem. Nylon 66 is a hygroscopic resin but to a lesser extent than Nylon 6. This may be an advantage as it improves flexibility and impact resistance of the parts, but in other cases, water absorption is likely to cause dimensional changes that are not always compatible with tight tolerance requirements. Furthermore, variation of mechanical characteristics resulting from water absorption will not always be acceptable.

Specific Notes for this Material: 30% mixed glass/carbon fibers; heat-stabilized; low electric resistivity; self-lubricating properties; high rigidity; low coefficient of linear thermal expansion.

Disclaimer from LATI: This document contains information based on average values as obtained from the results of laboratory tests and observations made on LATI materials. Tested materials were injection molded, used in their natural color, and conditioned in compliance with Standard ASTM D 618, procedure A. These values refer to LATI's best technical and scientific knowledge at the moment of testing and cannot be used as a basis for the development of applications. For a better assessment of the materials, you are kindly requested to contact LATI's technical or commercial offices, which are at your disposal and will supply detailed information on the most suitable characteristics for their intended use. With reference to DPR n.224 dated May 24, 1988, issued in accordance with EC Guide-lines 85/374, LATI Industria Termoplastici S.p.A. declines all responsibility arising from an improper use of the products described in this document.

All data provided by LATI.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.31 g/ccISO 1183
Linear Mold Shrinkage 0.0020 cm/cmLATI
Linear Mold Shrinkage, Transverse 0.0050 cm/cmLATI
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 190 MPaISO 527
Flexural Modulus 12.0 GPaASTM D790
Izod Impact, Notched 90.0 J/m
@Temperature 23.0 °C
ASTM D256
Charpy Impact Unnotched 4.00 J/cm²
@Temperature 23.0 °C
DIN 53453
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1000 ohmIEC 93
Dielectric Strength 2.50 kV/mm
@Thickness 1.00 mm
IEC 243-1
Comparative Tracking Index <= 100 VIEC 112
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 256 °CASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 - 290 °C
Mold Temperature 70.0 - 90.0 °C
Drying Temperature 80.0 - 100 °CTemperature can be reduced when using vacuum ovens.
Dry Time >= 3 hourDrying time can be reduced when using vacuum ovens.
 
Descriptive Properties
Heat Resistance - Ball Test (125°C)YIEC 335
Heat Resistance - Ball Test (165°C)YIEC 335
Injection Speedmedium
Needle Burner TestN1.47 mm
 N3.05 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLATI048 / 50046

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.