MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Go Yen Chemical GoyenchemAO-168 Antioxidant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CAS No. 31570-04-4

GoyenchemAO-168 Antioxidant is a hydrolytically stable phosphite processing stabilizer as a secondary antioxidant.

Applications:

  • polyolefins or olefin-copolymers :HDPE, LLDPE, PP, EVA, PC, PA.
  • engineering plastics :PBT, PET, styrenics
  • elastomers : PS, ABS, BR, SBS , tickifier resins, adhesives.

    Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.480 - 0.570 g/cc0.0173 - 0.0206 lb/in³
Density 1.03 g/cc0.0372 lb/in³
Volatiles <= 0.30 %<= 0.30 %
Molecular Weight 646.9 g/mol646.9 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 183 - 187 °C361 - 369 °F
 
Descriptive Properties
AppearanceWhite, non-flowing powder
Assay>99%
Composition<0.4%2,4-ditert-butylphenol
 <0.5%phosphate
Solubility<0.01 g/100g solutionMethanol
 <0.01 g/100g solutionWater
 0.1 g/100g solutionEthanol
 1 g/100g solutionAcetone
 11 g/100g solutionn-Hexane
 16 g/100g solutionCyclohexane
 30 g/100g solutionToluene
 34 g/100g solutionBenzene
 36 g/100g solutionChloroform
 36 g/100g solutionMethylene Chloride
 4 g/100g solutionEthyl aceta

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN509 / 266817

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.