MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI adhesives

Advanced Elastomer Systems Santoprene® 8281-35W237 Thermoplastic Rubber  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other melt processing techniques. Supplied as free-flowing pellets in 25 kilogram (55 pound) moisture barrier bags.

Features:

  • Non-hygroscopic product, requires little to no drying before processing
  • Neutral, easy coloring formulation
  • USP Class VI Certificate of Compliance
  • Drug Master File established with FDA

Product Notes: Values are for injection molded plaques, side gated.
82.6 mm x 117.5 mm x 3 mm

Information provided by Advanced Elastomer Systems.

Advanced Elastomer Systems is now a part of ExxonMobil. This grade was removed from the Advanced Elastomers Systems standard product line before the ExxonMobil acquisiton.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 35355 seconds; ASTM D2240
 40405 seconds, After oven air aging 168 hours @ 150°C; ASTM D2240
Tensile Strength at Break 1.86 MPa270 psiAfter oven air again 168 hrs. @ 150°C; ASTM D412
 3.10 MPa450 psiAcross flow; ASTM D412
Tensile Strength, Yield 1.00 MPa145 psiAt 100% elongation, across flow; ASTM D412
Elongation at Break 270 %270 %After oven air aging 168 hrs. @ 150°C; ASTM D412
 450 %450 %Across flow; ASTM D412
Tear Strength 3.68 kN/m21.0 pli212°F; ASTM D624
 12.1 kN/m69.0 pli73°F; ASTM D624
Compression Set 15 %
@Temperature 22.8 °C,
Time 612000 sec
15 %
@Temperature 73.0 °F,
Time 170 hour
Method B; ASTM D395
Tensile Set 5.0 %5.0 %ASTM D412
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -62.0 °C-79.6 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 177 - 232 °C351 - 450 °F
Drying Temperature 82.0 °C180 °FDesiccant Dryer
Dry Time 3 hour3 hourDesiccant Dryer
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Advanced Elastomer Systems Santoprene® 281-64 Thermoplastic Rubber
Dow Silastic® MDX4-4210 BIOMEDICAL GRADE ELASTOMER WITH CATALYST
Kraton® Kraton® G-2706 Styrene-based Biomedical Elastomer
Advanced Elastomer Systems Santoprene® 181-55 Thermoplastic Rubber
ExxonMobil Santoprene® 8281-35MED Thermoplastic Elastomer

PADW164 / 22882

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.