MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® 49H NT0745 PA66-I
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes: Vydyne 49H NT0745 is a general-purpose, impact-modified, high modulus PA66 resin. 49H NT0745 is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact strength. This resin offers a well balanced combination of engineering properties characterized by high melt point, good surface lubricity, abrasion resistance, resistant to most chemicals including motor oils, transmission fluids, lubricants and fuels.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/ccDAM; ISO 1183
Linear Mold Shrinkage, Flow 0.026 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.019 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 48.0 MPa50% RH; ISO 527-2
 70.0 MPaDAM; ISO 527-2
Elongation at Break 19 %DAM; ISO 527-2
 86 %50% RH; ISO 527-2
Tensile Modulus 1400 MPa50% RH; ISO 527-2
 2700 MPaDAM; ISO 527-2
Flexural Strength 30.0 MPa50% RH; ISO 178
 78.0 MPaDAM; ISO 178
Flexural Modulus 1200 MPa50% RH; ISO 178
 2600 MPaDAM; ISO 178
Izod Impact, Notched (ISO) 7.90 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 8.30 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 12.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
 12.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 20.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched NB
@Temperature -40.0 °C
50% RH; ISO 179/1eU
 NB
@Temperature -40.0 °C
DAM; ISO 179/1eU
 NB
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 NB
@Temperature -30.0 °C
DAM; ISO 179/1eU
 NB
@Temperature 23.0 °C
50% RH; ISO 179/1eU
 NB
@Temperature 23.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 7.60 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 8.90 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 9.20 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 11.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eA
 12.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 20.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 31.0 kV/mm
@Thickness 1.00 mm
DAM; IEC 60243
 34.0 kV/mm
@Thickness 1.00 mm
50% RH; IEC 60243
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 213 °CUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 67.0 °CUnannealed; DAM; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 280 - 310 °CInjection
Middle Barrel Temperature 280 - 310 °CInjection
Front Barrel Temperature 280 - 310 °CInjection
Nozzle Temperature 280 - 310 °CInjection
Melt Temperature 285 - 305 °CInjection
Mold Temperature 65.0 - 95.0 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 4.00 hourInjection
 
Descriptive Properties
AdditiveHeat Stabilizer
AppearanceNatural Color
FeaturesAbrasion Resistance
 Chemical Resistant
 Fast Molding Cycle
 Gasoline Resistant
 General Purpose
 Good Processability
 Good Toughness
 Heat Stabilized
 High Impact Resistance
 Impact Modified
 Oil Resistant
 Solvent Resistant
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE9232 / 287592

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.