MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lanxess Addocat® 1926 PU Catalyst/Activator
Categories: Other Engineering Material; Catalyst/Initiator

Material Notes: Addocat 1926 catalyses the gas formation and crosslinking reactions and is used exclusively for rigid polyurethane foam systems. As the product contains only 50% of active ingredient, it must be used at dosages of 2 - 6 p.b.w. , calculated on 100 p.b.w. polyether polyol. Addocat 1926 is particularly suitable for simple, yet accurate metering units as well as for automatic metering.

Function: Catalyst for the production of rigid polyurethane foams.

Applications:

  • Continuous and discontinuous production of foam sheets and sandwich panels.
  • Discontinuous heat/cold insulation of piping and refrigeration equipment.
  • On-site casting.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/cc
Water Absorption <= 0.50 %
Viscosity 15 cP
 
Thermal PropertiesOriginal ValueComments
Melting Point -62.0 °CFreezing Point
Boiling Point 150 °CInitial
Flash Point 44.0 °CDIN 51755
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
Amine number137-147 mg HCl/g
Appearanceclear, slightly yellowish liquid
Hydroxyl value190
Specifications0.46 p.b.w/1 p.b.wMDI basic value (NCO=31%)
 50 percentActive substance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY8189 / 208582

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.