MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Astro Met AmAlOx 68 Alumina - Aluminum Oxide
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: General Description:

AmAlOx 68 alumina (Astro Met Aluminum Oxide) is a high purity 99.8% aluminum oxide (alumina) ceramic which has been developed and optimized for maximum wear resistance and corrosion resistance. A high density, diamond like hardness, fine grain structure and superior mechanical strength are the unique properties that make AmAlOx 68 alumina the material of choice for a wide range of demanding applications. AmAlOx 68 alumina provides a cost-effective, engineered material solution in applications that require the optimum in wear resistance, corrosion resistance, high temperature stability, low thermal expansion, high stiffness to weight ratio, high dielectric strength and biocompatibility.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 3.93 g/cc
Water Absorption 0.00 %
Particle Size 4.0 µm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 2017
Modulus of Elasticity 393 GPa
Flexural Strength 382 MPa
Poissons Ratio 0.22
Fracture Toughness 5.00 MPa-m½
Shear Modulus 161 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 9.7
Dielectric Strength 230 V/milac-volts/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.20 µm/m-°C
@Temperature 25.0 - 1000 °C
Thermal Conductivity 260 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1700 °Cno load
 
Component Elements PropertiesOriginal ValueComments
Al2O3 99.8 %
 
Descriptive Properties
ColorWhite
Gas Permeation, %0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Materion Thermalox® 995 General Purpose 99.5% BeO
Nabaltec NABALOX® NO 201 Calcined Aluminum Oxide
CoorsTek AD-85 Alumina (nom. 85% Al2O3)
Mitsubishi Chemical Advanced Materials Ketron™ LSG PEEK-CLASSIX™ (white) Life Science Grade
Arkema OREVAC® 18921A Epoxide Modified Polyethylene

CASTR00 / 628

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.