MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Elastocon TPE Technologies Elastocon® 8088N Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Elastocon® 8088N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8088N is FDA compliant and well suited for consumer goods and industrial applications requiring U.V. stability. Elastocon® 8088N can be overmolded to polypropylene.

Information provided by Elastocon TPE Technologies, Inc. Elastocon® TPE Technologies has been acquired by Aurora Plastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.990 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.010 - 0.020 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90ASTM D2240
Tensile Strength, Yield 1446 psiASTM D412
Elongation at Break 463 %ASTM D412
100% Modulus 1.031 ksi
@Strain 100 %
ASTM D412
Compression Set 27 %
@Time 79200 sec
ASTM D395B
 
Processing PropertiesOriginal ValueComments
Feed Temperature 79.0 °C
Rear Barrel Temperature 350 - 380 °F
Front Barrel Temperature 360 - 390 °F
Nozzle Temperature 370 - 400 °F
Mold Temperature 70.0 - 100 °F
Back Pressure 50.0 - 100 psi
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
Injection RateFast

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elastocon TPE Technologies Elastocon® 8078NL Thermoplastic Elastomer
Elastocon TPE Technologies Elastocon® 8088BL Thermoplastic Elastomer
Elastocon TPE Technologies Elastocon® SMR1600 Thermoplastic Polyolefin Elastomer
Elastocon TPE Technologies Elastocon® SMR1555 Thermoplastic Polyolefin Elastomer
Denka REOMER G G8082 Thermoplastic Elastomer, For Injection Molding

PELASC18 / 81662

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.