MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite Durez® 31513 Phenolc Resin
Categories: Polymer; Thermoset; Phenolic

Material Notes: Durez® 31513 is a thermosetting phenol formaldehyde resin of the one-step type ( resole ), dissolved in MEK. Durez® 31513 is recommended for use in nitrile rubber solvent cements. 30 to 75 parts of resin per 100 parts of rubber are used depending on the degree of reinforcement, hardness or flexibility required in the adhesive film. Handling of the resin is much easier than standard solid resin because additional solvent can be added very easily. Strong bonds occur after the solvent has been eliminated and as they age, they become even stronger. Where increased heat resistance is a factor, cure temperatures oF120°C and higher are recommended. In many applications curing at room temperature is sufficient. Cements based on Durez® 31513 have a variety of uses, such as metal to metal adhesion, metalrubber bonding systems, brake lining bonding systems, shoe manufacturing and general adhesives.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 69 %
@Load 0.000750 kg,
Temperature 105 °C
1 hr; DCT 156.105
Viscosity Measurement 900DCT 61
 
Processing PropertiesOriginal ValueComments
Cure Time 55.0 sec
@Treatment Temp. 165 °C
DCT 162
 
Descriptive Properties
AppearanceLight yellow liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bakelite® PF 1141 Phenolic Formaldehyde Resin, High Surface Quality, Resistant to High Temperatures, Dishwasher Proof
Sumitomo Bakelite Durez® 17983 Phenolic Resin
Chemours Teflon® PFA Grade 940 HP Plus Extrusion and Molding Resin
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded

PSUMIT248 / 194053

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.