MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ Copolymer SLX2432T Polycarbonate (PC) (Americas)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors.

Features: Weatherable

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Density 1.20 g/ccISO 1183
Water Absorption 0.12 %
@Time 86400 sec
ASTM D570
Moisture Absorption 0.0200 %Injection Molding
 0.170 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.25 %ISO 62-1
Viscosity 9.0 cP
@Load 1.20 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 69.0 MPa50 mm/min; ISO 527
 72.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 65.0 MPa50 mm/min; ISO 527
 67.0 MPa50 mm/min; ASTM D638
Elongation at Break 110 %50 mm/min; ASTM D638
 110 %50 mm/min; ISO 527
Elongation at Yield 6.0 %50 mm/min; ASTM D638
 6.0 %50 mm/min; ISO 527
Tensile Modulus 2550 MPa50 mm/min; ASTM D638
 2550 MPa1 mm/min; ISO 527
Flexural Strength 105 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 105 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2500 MPa1.3 mm/min, 50 mm span; ASTM D790
 2500 MPa2 mm/min; ISO 178
Izod Impact Notched 700 JASTM D256
 98.0 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched 2600 J/mASTM D4812
Izod Impact, Notched (ISO) 25.0 kJ/m²80*10*3; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*3; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 30.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 15.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 77.0 JASTM D3763
 85.0 J
@Temperature -40.0 °C
ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 175 - 250 VUL 746A
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness >=1.50 mm
UL 746A
 30 - 60 sec
@Thickness >=3.00 mm
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
@Thickness >=1.50 mm
UL 746A
 15 - 30 arcs
@Thickness >=3.00 mm
UL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 66.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 66.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 64.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 64.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 130 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 130 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 116 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 118 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 135 °CRate B/50; ASTM D1525
 135 °CRate B/50; ISO 306
 137 °CRate B/120; ISO 306
UL RTI, Electrical 110 °CUL 746B
UL RTI, Mechanical with Impact 110 °CUL 746B
UL RTI, Mechanical without Impact 110 °CUL 746B
Flammability, UL94 V-2
@Thickness >=1.50 mm
UL 94
Oxygen Index 38 %ISO 4589
Glow Wire Flammability Index 960 °C
@Thickness 1.60 mm
IEC 60695-2-12
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.59ASTM D542
Haze 0.80 %
@Thickness 2.54 mm
ASTM D1003
Transmission, Visible 84 %
@Thickness 2.54 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 275 - 295 °C
Zone 2 265 - 290 °C
Zone 3 280 - 300 °C
Melt Temperature 280 - 300 °CInjection Molding
Mold Temperature 70.0 - 95.0 °C
Drying Temperature 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 48.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80422 / 288369

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.