MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Abatron AboCoat 8006-3/8606-3 Clear Versatile Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Clear epoxy protective and dielectric coatings. For spraying, brushing or rolling on metal, concrete, masonry, wood, fiberglass and most surfaces. Good adhesion, flexibility, hardness, water and chemical resistance.

Suggested Uses: Heavy-duty all-purpose protection against water, alkalis, diluted acids, common solvents, corrosion, wear. Corrosion inhibition also on tightly bound rust. Good salt spray resistance in marine and industrial applications. Concrete, wood and metal floors coating. Brushing on moist or wet surfaces tends to emulsify water, which then evaporates with solvent. Protection of wooden furniture in plants, laboratories, commercial kitchens, hospitals. Most effective for protection of all kinds of electric and electronic components.

Processing:

Ratio by volume: 1/1 AboCoat/AboCure

Cure Schedule: Room temperature cure 4-6 hours for handling, 3-4 days for full physical properties, and 6-8 days for full chemical properties. High temperature cure 25 minutes at 200°F, 15 minutes at 250°F, 10 minutes at 300°F, or 5 minutes at 350°F.

Information provided by Abatron.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.03 lb/gal
Solids Content 47.4 %Total
Viscosity Measurement 25secs., #4 Ford cup.
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD >= 60 %Direction not specified
Impact Test 160 in-lbForward/reverse
 
Optical PropertiesOriginal ValueComments
Gloss 60 %3 mils, 48 hours
Transmission, Visible 90 %clear; thickness not quantified
 
Processing PropertiesOriginal ValueComments
Dry Time 3.00 hour
@Temperature 23.0 °C
Pot Life 60 - 75 min
Shelf Life >= 12.0 Month
 
Descriptive Properties
AdhesionExcellentCrosshatch
Induction Period40-60 minutes
Mandrel FlexibilityPasses 1/8"
Pencil Hardness3Overnight at room temperature
 4H7 days

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PABKW012 / 22053

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.