Uncured silicone rubber with a minimum thickness of 0.0035 in. (0.0889 mm)/ 0.008 in. (0.2 mm) Prime Coated 7628 Fiberglass/Uncured silicone rubber with a minimum thickness of 0.0035 in. (0.0889 mm); 0.003 in. (0.08 mm) polyethylene interleave; overall thickness 0.015 in ±0.0015 (0.381 mm ± 0.038). The shelf life is defined as the duration of time for which the product will meet the physical requirements outlined below. It does not guarantee the product’s usefulness in all applications. Color: Red. Weight: 549.3 g/m² ± 50.86 (16.2 oz./yd.² ± 1.5). Shelf Life: 6 months from date of manufacture at 23.8°C (75°F). Cure Time: 0.25 hours. Post Cure: 204°C (400°F), for 2 hours. Information provided by the manufacturer, Arlon Silicone Technologies Division. Information provided by Arlon Silicone Technologies; now a part of Rogers Corporation. |