MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilamid® LV-15H nat PA12-GF15
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 20% Glass Fiber Filled

Material Notes: Product description: Grilamid LV-15H is a 15% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile:
  • very low water absorption
  • good dimensional stability
  • very high elongation
  • good chemical resistance
  • good UV stability
  • high impact strength
Grilamid LV-15H is suitable for the manufacturing of technical parts in the application fields of:
  • Electrical and electronic components
  • Automotive
  • Safety parts
  • Mechanical engineering
  • Domestic appliances
  • Analytical and mecical devices
  • Sports & leisure goods

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccDry; ISO 1183
Water Absorption 1.3 %Sim. to ISO 62
Moisture Absorption 0.800 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 74
@Time 15.0 sec
Conditioned; ISO 868
Tensile Strength at Break 70.0 MPaConditioned; ISO 527-1/-2
 80.0 MPaDry; ISO 527-1/-2
Elongation at Break 8.0 %Dry; ISO 527-1/-2
 10 %Conditioned; ISO 527-1/-2
Tensile Modulus 3000 MPaConditioned; ISO 527-1/-2
 3500 MPaDry; ISO 527-1/-2
Charpy Impact Unnotched 75.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
 75.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 15.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Strength 35.0 kV/mmConditioned; IEC 60243-1
Comparative Tracking Index 600 VConditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 40.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°CISO 11359-1/-2
Melting Point 178 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 120 °CLong Term; ISO 2578
 150 °CShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 150 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 80.0 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAutomotive electr. and electronics, lighting
 Compressed air systems
 Cooling and climate control
 Fuel systems
 Hydraulic systems
 Powertrain and Chassis
Electricals & ElectronicsConnectors
 Electrical appliances
FormGranules
Industry & Consumer goodsHousewares
 Hydraulics & Pneumatics
 Mechanical Engineering
 Medical devices
 Power transmission
 Sanitary, water and gas supply
 Sports & Leisure
 Tools & Accessories
ProcessingInjection Molding
Product AttributesHydrolysis resistant
Special CharacteristicsHigh impact or impact modified
 Improved heat resistance
 Improved UV resistance (outdoor use)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
301 Stainless Steel
Multibase TPSiV® 4000-70A Thermoplastic Silicone Vulcanizate
Alclad Aluminum 6061-T6, T651
Alliance N-42H Neodymium Iron Boron Magnetic Material
410 Stainless Steel

PGRH071 / 156780

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.