- Specially formulated for battery soldering applications.
- Wide active temperature range.
- Completely free of Zinc Chloride and other chlorides.
- High fluxing activity.
- Low VOC Emissions.
Description: Superior No. 555C Battery Flux is specially formulated as a low VOC, non-flammable product for the Cast-on-Strap (CoS) manufacturing process in high concentrate formulation. This flux contains no chlorides, heavy metals, or organic acids that could affect the long-term life of batteries. Additional formulation advantage of this flux is the wide window of operation at various temperatures and line speeds. Superior No. 555C Battery Flux remains consistently active to produce strong burn-in cast bonds and allow the flux to be used in low temperature operations due to potential cracking of straps or to be used in high temperature applications to accommodate the larger mass platesInformation provided by Superior Flux |