MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CeramTec Ceramtape GC Glass Ceramic
Categories: Ceramic; Glass; Glass Ceramic

Material Notes: LTCC (Low Temperature Cofired Ceramic) is a new type of ceramic film developed by CeramTec AG's Electronics division. With the aid of these ceramics and their almost shrinkage-free sintering process, highly complex multilayer assemblies for electronic applications are possible. Apart from the automotive sector, LTCC is also ideally suited for the up-and-coming Bluetooth applications, medical apparatus, and consumer electronics. In the automotive sector, it is used for motor-management and ABS-systems. Ceramtape GC is a glass ceramic made of alumina and anorthite.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 1.63 - 1.93 g/ccGreen
Density 2.87 - 2.97 g/ccFired
Thickness 40.0 - 60.0 micronsPET
 324 - 396 micronsBlank on PET
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength >= 170 MPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 7.3 - 8.5
@Frequency 1e+6 Hz
Dielectric Strength >= 100 kV/mm
Dissipation Factor <= 0.0020
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.90 - 5.70 µm/m-°C
Thermal Conductivity 1.20 - 3.20 W/m-K
Shrinkage 17.5 - 18.5 %2-layer Laminate; z-direction
 20.5 - 21.5 %2-layer Laminate; x-direction
 20.9 - 21.9 %2-layer Laminate; y-direction
 
Descriptive Properties
Cooling Rate (K/min)1 to 6Firing Conditions
Dwell Time at Peak Temperature (min)10 to 40Firing Conditions
Heating Rate (K/min)1 to 4Firing Conditions
Laminating Pressure (kg/cm³)50-130
Laminating Temperature (°C)30-80
Laminating Time (min)0.5-3
Peak Temperature (°C)880-920Firing Conditions

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schott KZFS12 Glass
Schott AF 45 Thin Borosilicate Glass
Schott Glass 8241 Alkaline Earth Aluminosilicate Glass
Quartzite
Accuratus MACOR Machinable Glass Ceramic

CCERA969 / 107569

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.