MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bostik Pure Silicone 100% Silicone Sealant
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Bostik Pure Silicone Sealant is a specially formulated, one-component, 100% silicone sealant for on a variety of substrates such as ceramic tile, slate, wood, metal, glass, fiberglass, laminate, plastic. For use as a flexible barrier between horizontal and vertical surfaces or any other changes in plane, expansion joints in non-traffic areas, fixtures, tub surrounds, sinks, toilets, vanities, electrical plumbing penetrations, floors, walls, ceilings, spas and steam showers.

Features & Benefit:

  • 100% Silicone for use in interior, exterior, wet and dry installations.
  • For use in expansion joins in non traffic areas
  • Superior elongation and flexibility for use in change of plane and joint applications.
  • Meets ASTM C920; Type S; Grade NS; Class 25; Use NT, G, A and O

    Information provided by Bostik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3030ASTM D2240
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -65.0 °C-85.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature -34.4 - 54.4 °C-30.0 - 130 °FApplication
Tack-Free Time 10.0 - 20.0 min0.167 - 0.333 hourASTM D2377
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Tooling Time5-10 mins

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade
Chemical Concepts Chem-Set™ RTV118S Silicone Sealant
Momentive Performance Materials TSE392 One Component RTV Adhesive Sealant/Coating, Clear/White
Dow 1437 INDUSTRIAL SEALANT AND ADHESIVE
CHT Group QSil 550SB QSI Quantum Silicones Self-Priming Silicone Potting Material

PBOSTK001 / 191537

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.