MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PSM Industries Ferro-TiC® C Medium Alloy Tool Steel
Categories: Ceramic; Carbide; Metal; Ferrous Metal; Alloy Steel; Medium Alloy Steel; Tool Steel

Material Notes: Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.

Excellent vibration dampening in the annealed condition, excellent cryogenic properties. Replaces A-2 tool steel. Highly Magnetic.

    Ferro-TiC® Unique Characteristics
  • Provides the lightweight, size, stability, and hardness
  • Virtually porosity free - significantly better than the A1 ASTM B-276-79 Standard
  • Low specific mass. Ferro-Tic® is 10-20% lighter than its steel counterpart and about 50% lighter than tungsten carbide
  • 10 times the wear resistance of tool steels
  • Economical fabrication (conventionally machinable in the annealed stage by milling and turning, conventionally heat treatable to achieve high hardness)
  • 50-90% less linear size change in heat treat than tool steels

Information Provided by Ferro-TiC®, a division of PSM Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.60 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 44Annealed
 70Hardened
Flexural Strength 216000 psiTransverse Rupture
Compressive Strength 520 ksi
Charpy Impact Unnotched 26.92 ft-lb/in²
 
Thermal PropertiesOriginal ValueComments
CTE, linear 1.96 µin/in-°F
@Temperature 21.1 - 191 °C
Maximum Service Temperature, Air 375 °F
 
Descriptive Properties
Carbide (Vol. %)45
Linear Size Change Thru Heat Treat %0.048
Thermal Shock (No. Cycles)5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PSM Industries Ferro-TiC® CM High Chrome Tool Steel
ASTM A353 Alloy Steel
PSM Industries Ferro-TiC® MS-5A Age Hardenable Martensitic Stainless Steel
PSM Industries Ferro-TiC® CM-25 High Chrome Tool Steel
PSM Industries Ferro-TiC® PK Maraging Steel

NPSM016 / 93207

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.